SUS304LN (18Cr-8Ni-N-Low C) adds N to the SUS304 steel, imparting the same properties as the original. Its applications are similar to those of SUS304N1 steel, but it offers superior intergranular corrosion resistance. SUS304LN corresponds to GB 00Cr18Ni10N and German DIN X2CrNiN1810.
Material Name: Austenitic Stainless Steel
Grade: SUS304LN
Standard: JIS (G 4303 Steel Bar)
Carbon C: ≤0.03
Silicon (Si): ≤1.00
Manganese (Mn): ≤2.00
Phosphorus P: ≤0.045
Sulfur: ≤0.030
Chrome (Cr): 17.00~19.00
Molybdenum (Mo): -
Nickel (Ni): 8.50~11.50
Copper: Cu
Nitrogen N: 0.12~0.22