Infrared High-Temperature Infrared Radiation Coating Instructions
Xuchang Infrared Research Institute has successively undertaken national, provincial, and municipal projects over the years.
Over 40 advanced research projects, with more than a dozen awards at various levels
Research achievements. Among them, the infrared non-ferrous metal melting technology.
Technology, infrared ceramic tunnel kiln, direct-heat infrared radiation
Sheet, high-temperature infrared radiation coatings, and other products. Infrared skin
Hair dryer, infrared electrostatic flocking drying system
Portable and transferable flocking machines have won the Henan Province Science and Technology Achievement Award
Second Prize, Provincial/Municipal High-Tech Products, National Real
Utilizing new patented and invention patents. Additionally“Solar Energy
Central Heating Project” 、“Infrared radiation pipe heating unit
Place”、“Rapid Infrared Radiation Heater”N/A
City Science and Technology Achievement Award Second Prize. Infrared Automatic Temperature Control Furnace,
Direct-heat infrared componentsXWGTModel High Temperature Red
Outward radiation paint88Named as Henan Province's Energy Conservation Recommendation Yearly
Project, Third Prize of Xuchang City for Science and Technology Progress.2002Year
We have developed a nano-low-temperature infrared radiation coating.
Material.
XWGTHigh-temperature infrared radiation paint, odorless
Harmless to humans, non-polluting, long shelf life, good adhesion, easy to install, and simple to operate. Its main performance features are as follows:
Fusibility temperature:1350℃
Hemispherical Reflectance:≥0.88
Shelf Life:18Over a month
1Pre-treatment for furnace and kiln coating
Old kilns: Remove the refractory lining material surface
Nodules, float layers, etc., if the refractory surfacejDry
Dry, lightly mist with water before painting for slightly moistened surface.
Brush or spray on.
2New Kiln: In principle, the surface of the refractory lining can
Direct spray application, if conditions permit, new establishment
Furnaces can also be parked2-3Aftertreatment, ready for moisture adsorption
Apply paint (spray) after shipment.
2Spraying:
Before use, mix the adhesive binder and powder by weight.
Ratio6:4Thoroughly mix until well blended, restoring to the original adhesive state
Body condition, construction should be carried out immediately after paint mixing is completed.
2>Transfer the paint to the spray equipment container, add
After mixing with an adequate amount of water, apply evenly. The coating thickness is generally
No more than1.0mmFirebrick and refractory concrete
Apply a slightly thicker coat, depending on the furnace material and usage time.
The differences are in the spray per square meter.0.5-2kgPlease provide the Chinese content you would like translated into American English.
Adequate.
3Brush coating:
1>Brush coating is suitable for smaller furnaces and furnace wall geometries.
Complexly shaped furnace.
2>On the surface of furnace refractory materials, use a brush to apply from above
Brush paint from bottom to top, left to right, and then horizontally and vertically
Apply several coats, then allow to dry naturally or
4Curing and hardening of the coating:
Coating dries within half a day, depending on weather conditions, during the dry season.
Heat and, if conditions permit, naturally dry.2-3Day, or
Low Temperature150-200℃Below roasting2-3Hourly, coating
The construction will be even more robust. Then, the furnace can be heated according to the normal heating curve.
Line is heated up.
Color Type
Black, Charcoal Green, Iron Red
Black, Olive Green, Rust Red
Black, Iron Red
Black, Ferric Red
Charcoal gray
Note:1All the above infrared radiation coating fillers use zirconium ceramic powder.