TNL coating characteristics: excellent heat resistance, resistance to alternating cold and hot temperatures, long-term temperature resistance of 300 ℃, acid and alkali resistance, chemical atmosphere and weather aging resistance, water resistance, moisture resistance, impermeability and electrical insulation properties. It belongs to the cross-linked room temperature self drying curing coating, with fast drying speed and easy construction.
Usage: This product is specifically designed for the outer walls of blast furnaces, chimneys, flues, floodways, exhaust pipes, hot gas pipelines of blast furnaces, heating furnaces, and other equipment that require high temperature corrosion protection on metal surfaces.
Main technical indicators:
The shear bond strength at room temperature is ≥ 2.5Mpa,
After soaking in room temperature water for 15 days, the shear bond strength is ≥ 2.4Mpa,
After drying at 280 ° Cx4, the shear bond strength is ≥ 2.3Mpa,
After drying at 300 ° Cx4, the shear bond strength is ≥ 2.3Mpa,
Soaking in 40% H2SO4 at 80 ° C for 15 days, the shear bond strength is ≥ 2.3Mpa, and the tensile bond strength at room temperature is ≥ 2.4Mpa,
Operating temperature ≥ 180 ° C
Packaging specification: 20KG/drum