2011 Prestressed Pipe Grouting Material for Highway_SupplyPro Co., Ltd._Guangdong Shijia Gaojian Building Materials Technology Co., Ltd. 
在线客服 在线客服邀请中...
关闭

您好,现在客服正邀请与您通话,请留下您的联系方式,客服将尽快与您取得联系。

 点击提交代表您同意《服务条款》《隐私政策》
Guangdong Shijia Gaojian Building Materials Technology Co., Ltd.

High-strength non-shrink grouting material, high-strength polymer mortar, bea...

Consultation Hotline
13829788227

News Center Co., Ltd.

Product Categories
Home > SupplyPro Co., Ltd. > 2011 Prestressed Pipe Grouting Material for Highway
2011 Prestressed Pipe Grouting Material for Highway
品牌: ShiJia Solid Construction
Water-to-gel ratio:
Initial setting: ≥5h
Final Set: ≤24
单价: 980.00/tons
最小起订Quantity: 1 tons
供货总Quantity: 9999 tons
有效期至: 长期有效
最后更新: 2022-12-22 14:42
 
详细Info

SJ-61 Prestressed Pipe Grouting Material

Product Description

1. Product Application Scope

This product meets the requirements of the "JTG/T F50-2011 (Technical Specifications for Construction of Highway Bridges and Culverts)" for high-performance grouting materials for prestressed voids.

Section II: Application Fields

1. Prestressed concrete beam pipe grouting  2. Equipment foundation, auxiliary rods, and other component grouting

3. Nuclear Power Plant Shell Grouting  4. Concrete Drainage, Crack and Hole Repair

III. Performance Specifications:

ProjectPerformance specificationsInspection and Testing Methods Standard

Water-to-Binder Ratio (%)0.26~0.28Cement standard dosage water content, setting time. Stability testing methods (GB/T1346)

Setting Time (h)Initial setting≥5 

 Final Solidification≤24 

Flowability (25℃) (s)Initial liquidity10~17JTG/T F50-2011 Appendix C3

 30-minute fluidity10~20 

 60-minute flow point10~25 

Water Permeability (%)24-hour moisture regain rate0JTG/T F50-2011 Appendix C4

 3H wire moisture content0JTG/T F50-2011 Appendix C5

Pressure Drop Rate (%)0.22 MPa (when the bore vertical height is 1.8 m)≤2.0JTG/T F50-2011 Appendix C6

 0.36 Mpa (when the hole channel vertical height is not less than 1.8 meters)  

Free Water Content (%)3h0~2JTG/T F50-2011 Appendix C4

 24h0~3 

FulfillmentQualifiedJTG/T F50-2011 Appendix C7

Compressive Strength (Mpa): 3d3d20Cement Aggregates Strength Testing Method (ISO Method) (GB/T 1761)

 7d≥40 

 28d≥50 

Flexural Strength (Mpa) 3d3d≥5

 7d≥6 

 28d≥10 

Corrosion effect on rebarNo rust(Concrete admixture) (GB8076)

 