300℃~1000℃Series Infrared Radiation Paint Application Instructions
I. Main Ingredients
Modified silicone resin, zirconium ceramic powder, thickeners, etc.
II. Features and Applications
The coating is a functional coating.,可直接 applied to the surface of the heating element to enhance its infrared radiation capability. It can also be coated onto the heated object to improve its absorption of infrared radiation energy. Construction Reference:
1Coating prior to applicationbStir thoroughly. If any foreign impurities are present, filter them out before use.
2Coated substratebRemove oil stains and then proceed with sandblasting (can also be)60-80#Sandpaper finishing, followed by spraying.
3Construction should be done by spraying, and manual brushing is also acceptable. Viscosity is generally15~20sIf necessary, you can thin out the paint if it's too thick.X-13Organosilicone paint thinner (diphenyl) diluted, coating thickness at70~100 μm。
4After spraying, leave to dry at room temperature.30After a few minutes, then gradually increase to room temperature and into the oven.300℃Baking30Cures in minutes.
V. Storage and Transportation
1The product is sealed and stored in a dry, well-ventilated warehouse with storage temperatures at35℃Below.
2Protect from direct sunlight, keep away from fire sources and heat, shelf life from the date of manufacture180Day, after the storage period, inspection can be conducted. If it meets the requirements, it can still be used.
3The product should be protected from rain and direct sunlight during transportation and comply with the relevant regulations of the transportation department.