Surface Treatment Requirements:
Process Flow: Rough Casting → Degreasing → Rust Removal → Surface Adjustment → Phosphating → Drying → Electrostatic Powder Coating → Curing → Packaging
2. Surface treatment uses electrostatic powder coating with epoxy resin, with a coating thickness of 60~80 micrometers.
3. The electrostatic powder coating adhesion meets the standard requirements.
4. Hardness (wear resistance) is over 100 times that of ordinary nitrocellulose paint, meaning it shows no scratches after a 2H pencil test.