The cast iron platform has undergone two manual treatments (manual annealing at 600-700 degrees and natural aging for 2-3 years), and the accuracy of using this product is stable. The raw material content and ingredients are added according to the following standards (%): carbon content: 3.1-3.4, manganese: 0.6-0.9, silicon: 1.5-2.0, sulfur<0.12, phosphorus<0.3.