- AllProduct Category
-
Brass Products
Brass Products
Brass Products
Brass Tube Coils
Lead Sheets
Lead Sheeting
Lead Rod


详情描述
Specializing in the sale of copper strips, bronze strips, and brass strips. High quality, competitive prices, stock availability, and same-day shipment.
Conductive copper busbar (conductive copper bar)
1) Production Grades: T1, T2, TU1, TU2; chemical composition follows GB/T5231-2001 standard.
The main component of copper busbars is: Main Components of Conductive Copper Bars as shown in Table 1.
Copper Bars T1, T2, TU1, TU2
Cu+Ag 99.95 99.90 99.97 99.95
2) Product Status: Table 2 - Conductive Copper Busbar Product Status
Product Name & Code Status Symbol Supply Method
Copper Busbars (TMR) - Soft R Rolling Supply
Copper busbar (TMY) Hard-state Y-shaped bar supply
3) Product size range: 1. Conductive copper bar cross-section
Thickness a, Width b, Radius of Curvature r
Copper busbar current-carrying capacity table:
National Standard Copper Busbar Current Load Estimation Method: - Estimation Method: Single copper busbar current load = width (mm) x thickness coefficient - Double busbar current load = width (mm) x thickness coefficient x 1.5 (experience coefficient) - Copper and aluminum busbars can also be calculated by area, typically copper at 5-8A/square, aluminum at 3-5A/square. - Common Copper Busbar Current Load Calculation: - At 40°C, copper busbar current load = width x thickness coefficient - Width (mm); thickness coefficient for 12mm thick busbar is 20; for 10mm thick, it's 18; and so on: [12-20, 10-18, 8-16, 6-14, 5-13, 4-12]. - Double-layer copper busbar [40°C] = 1.56-1.58; Single-layer copper busbar [40°C] (determined by cross-sectional size); 3-layer copper busbar [40°C] = 2; 4-layer copper busbar [40°C] = single-layer copper busbar [40°C] x 2.45 (not recommended, use shaped busbars instead); copper busbar [40°C] = copper busbar [25°C] x 0.85; aluminum busbar [40°C] = copper busbar [40°C] / 1.3. - For example, the current load of TMY100*10 is: - Single-layer: 100 x 18.8 = 1800(A) [manual check = 1860A]; - Double-layer: 2(TMY100*10) current load = 1860 x 1.58 = 2940(A) [manual check = 2942A]; - Triple-layer: 3(TMY100*10) current load = 1860 x 2 = 3720(A) [manual check = 3780A]. - All calculations are precise and very close to the manual data.