1-200m³ Stainless Steel Lined PTFE Storage Tank_SupplyPro Co., Ltd._Wuxi Huashun Anticorrosion Container Technology Co., Ltd. 
在线客服 在线客服邀请中...
关闭

您好,现在客服正邀请与您通话,请留下您的联系方式,客服将尽快与您取得联系。

 点击提交代表您同意《服务条款》《隐私政策》
13921511789
 

Product Categories
  • No Category

Contact Information
  • Contact person:张总
  • Telephone:13921511789
  • Mobile:13921511789
  • Address:38 Luoyang North Road, Shuangmiao Village, Luoshi Town, Wuxi City, Huishan District
Home > SupplyPro Co., Ltd. > 1-200m³ Stainless Steel Lined PTFE Storage Tank
1-200m³ Stainless Steel Lined PTFE Storage Tank
品牌: Huashun
Origin: Wuxi
Customized Processing: Is
Performance: Corrosion-resistant, leak-proof, non-flaking
单价: 电议
最小起订Quantity:
供货总Quantity:
有效期至: 长期有效
最后更新: 2025-05-09 14:22
 
详细Info

Pre-treatment

The inner surface of the lining equipment is first degreased with solvents and dried, followed by sandblasting with 46# steel shot. The sandblasted surface is then cleaned and dried with trichloroethylene.

Surface Paint Treatment

Section 3: Adhesive Coating

The product is evenly coated with a special adhesive inside, and the back of the composite board is also coated with adhesive, followed by positioning and attaching the board accordingly.

Four, Paste

After aligning the adhesive-coated composite panels in their designated positions, apply them first. Then, use local heating and rolling to expel the air trapped in between, ensuring a tighter fit for the 3mm or 4mm polytetrafluoroethylene sheets.

Section 5: Weld Seam

Once the composite boards are fully bonded, use a professional notching machine to cut "V" shaped long grooves at the joint between the two boards, and clean out any impurities from the gaps.

Welding

Utilize imported high-temperature welding torches with Φ3.5mm PFA welding rods. Weld the two composite panels together in the middle of the grooved seam, ensuring there are no impurities, bubbles, or incomplete welds. After the overall welding is completed, use a pinhole tester to test at 15,000 volts to check for any micro-pores and make necessary repairs. Upon completion of the inspection, use an imported grooving machine to flatten any protruding welding rods on the composite panel. Then, reinforce the original welding rods with a 20mm-wide welding strip to ensure the welds are secure and free of micro-pores. Finally, test for pinholes using 30,000 volts to further confirm the welding integrity.

Section 7: Inspection